Make four round coasters from a single batch. Leave two clear and colour the other two with an epoxy-compatible pearlescent mica powder. Using the same mould and pour depth lets you see how the pigment changes the colour and the way the piece catches the light. Make the set for yourself or as a gift. The same comparison works for pendants, keyrings and small decorative pieces.
What to buy for a first project
- Casting resin and its hardener. Check that the chosen mould depth and batch size fit the instructions.
- A ready-made silicone mould. Four identical cavities make the results easy to compare. Set the mould on a level surface.
- Mica powder rated for the epoxy. Check the resin and pigment instructions for the allowed dose and when to add it.
- Scales or measuring cups, two dry cups and a mixing stick. Prepare ventilation and protective equipment as required by the safety data sheets for both materials.
Four steps from mixing to comparing the results
- Calculate the amount. Four cavities of 9 cm diameter and 6 mm fill depth take about 153 mL before allowance. Dry the mould completely and set it flat.
- Measure and mix A and B. Follow the product's own ratio and units. Mix as instructed, including material at the sides and the base of the cup. Transfer to a second cup if the manufacturer recommends that method.
- Split the mix into two portions. Do this if your instructions allow mica to be added to the combined A+B mixture. Add a small permitted dose of pigment to one portion and leave the other clear. Record the portion weight and pigment dose to reproduce the shade. Fill two cavities with each mix to the same depth and work within the specified time.
- Let the resin cure. Protect the mould from dust and keep it at the specified temperature. Demould when the instructions allow and assess after full cure. Set the pairs against a light and dark background and tilt them towards side light. Compare how much of the background you can see and how the shimmer changes.
What if there are bubbles or the surface feels tacky?
Air can be introduced by mixing or by filling the mould too quickly. On the next try, check that the mould is dry and change one factor, such as the pouring speed. If the entire surface stays tacky past the specified cure time, verify the ratio, mixing and temperature. If only the mica pair is affected, check the pigment dose and compatibility. Handle uncured material according to the safety data sheet.
What to try next
For a translucent tint, look for an epoxy colourant intended for transparent effects. For a solid background, try a compatible opaque paste. Record each recipe and test it at the intended thickness before making a full set. Check the specific product's documentation for hot items or food contact.